First he tore out the old plywood deck. He checked the stringer to make sure they were still good.
He installed a new plywood deck.
And covered it with knitted fiberglass, GP resin and ISO/NPG Gel coat. The boat deck looks great.
Here is a list of the materials and supplies that Charles used.
Type 1708 Knitted Fabric, 25.3oz. X 50", +/-45 17 oz w/ 3/4oz. Mat - Yards
Ortho General Purpose Laminating Resin - 5 Gallon
Deluxe Aluminum Roller - 1" x 6"
White 1100 Gel Coat - No Wax- Gallon
White Gel Coat WITH WAX - Gallon
Charles added sand to the White Gel coat with wax to give the surface a non-skid texture. He is extremely please with the job he did. This was his first ever fiberglassing attempt.